ELECTRON MICROSCOPY


Sample

Hemagglutinin CA09 homotrimer bound to anchor fab

Specimen Preperation
Sample Aggregation State PARTICLE
Vitrification Instrument FEI VITROBOT MARK IV
Cryogen Name ETHANE
Sample Vitrification Details ?
3D Reconstruction
Reconstruction Method SINGLE PARTICLE
Number of Particles 90138
Reported Resolution (Å) 2.9
Resolution Method FSC 0.143 CUT-OFF
Other Details ?
Refinement Type
Symmetry Type POINT
Map-Model Fitting and Refinement
ID 1
Refinement Space ?
Refinement Protocol ?
Refinement Target ?
Overall B Value ?
Fitting Procedure ?
Details ?
Data Acquisition
Detector Type FEI FALCON IV (4k x 4k)
Electron Dose (electrons/Å2) 44.94
Imaging Experiment
Date of Experiment ?
Temprature (Kelvin)
Microscope Model TFS GLACIOS
Minimum Defocus (nm) 800
Maximum Defocus (nm) 1500
Minimum Tilt Angle (degrees) ?
Maximum Tilt Angle (degrees) ?
Nominal CS 2.7
Imaging Mode BRIGHT FIELD
Specimen Holder Model FEI TITAN KRIOS AUTOGRID HOLDER
Nominal Magnification 190000
Calibrated Magnification ?
Source FIELD EMISSION GUN
Acceleration Voltage (kV) 200
Imaging Details ?
Imaging Experiment
Task Software Package Version
PARTICLE SELECTION cryoSPARC v4.1.2
MODEL FITTING Coot ?
MODEL REFINEMENT PHENIX ?
RECONSTRUCTION cryoSPARC v4.1.2
Image Processing
CTF Correction Type CTF Correction Details Number of Particles Selected Particle Selection Details
NONE ?