8SP8

ELECTRON MICROSCOPY


Sample

sample 1

Specimen Preperation
Sample Aggregation State PARTICLE
Vitrification Instrument FEI VITROBOT MARK IV
Cryogen Name ETHANE
Sample Vitrification Details ?
3D Reconstruction
Reconstruction Method SINGLE PARTICLE
Number of Particles 213249
Reported Resolution (Å) 2.79
Resolution Method FSC 0.143 CUT-OFF
Other Details ?
Refinement Type
Symmetry Type POINT
Map-Model Fitting and Refinement
ID 1
Refinement Space REAL
Refinement Protocol ?
Refinement Target ?
Overall B Value ?
Fitting Procedure ?
Details ?
Data Acquisition
Detector Type GATAN K3 (6k x 4k)
Electron Dose (electrons/Å2) 60
Imaging Experiment
Date of Experiment ?
Temprature (Kelvin)
Microscope Model TFS KRIOS
Minimum Defocus (nm) 800
Maximum Defocus (nm) 2000
Minimum Tilt Angle (degrees) ?
Maximum Tilt Angle (degrees) ?
Nominal CS 2.7
Imaging Mode BRIGHT FIELD
Specimen Holder Model ?
Nominal Magnification ?
Calibrated Magnification ?
Source FIELD EMISSION GUN
Acceleration Voltage (kV) 300
Imaging Details ?
Imaging Experiment
Task Software Package Version
PARTICLE SELECTION cryoSPARC ?
IMAGE ACQUISITION SerialEM ?
CTF CORRECTION cryoSPARC ?
MODEL FITTING Coot 0.9.8.1
MODEL REFINEMENT PHENIX 1.19.2
INITIAL EULER ASSIGNMENT cryoSPARC ?
FINAL EULER ASSIGNMENT cryoSPARC ?
CLASSIFICATION cryoSPARC ?
RECONSTRUCTION cryoSPARC ?
Image Processing
CTF Correction Type CTF Correction Details Number of Particles Selected Particle Selection Details
NONE ?